Technical Data for Secure Set - 4
| TEST METHOD | PROPERTIES |
| |
| Wt./Gal. A | Brookfield | 10.5 lb. |
| Wt./Gal. B | Brookfield | 10.0 lb. |
| Viscosity A | Brookfield | 100 cps@77°F |
| Viscosity B | Brookfield | 475 cps@77°F |
| Density (set) | ASTM D-1622 | 4 lbs./cu. ft. |
| Expansion Ratio | ASTM D-1622 | 18:1 |
| K Factor | | |
| fresh | ASTM D-518 | 0.14 |
| aged | | 0.145 |
| Compressive Strength | ASTM D-1621 | 85 psi |
| Tensile Strength | ASTM D-1623 | 130 psi |
| Dimensional Stability | 158 F-97% RH for 2 weeks | <1% |
| Water Absorbtion | ASTM D-2842 | <0.5% |
| Water vapor Transmission | ASTM C-355 | 0.5 perms |
| Max Application Temperature | | 250°F |
| Mixing Ratio by Volume | | 1:1AB |
Technical Data for Secure Set - 6
| TEST METHOD | PROPERTIES |
| |
| Wt./Gal. A | Brookfield | 10.5 lb. |
| Wt./Gal. B | Brookfield | 10.0 lb. |
| Viscosity A | Brookfield | 100 cps@77°F |
| Viscosity B | Brookfield | 475 cps@77°F |
| Density (set) | ASTM D-1622 | 4 lbs./cu. ft. |
| Expansion Ratio | ASTM D-1622 | 13:1 |
| K Factor | | |
| fresh | ASTM D-518 | 0.14 |
| aged | | 0.145 |
| Compressive Strength | ASTM D-1621 | 140 psi |
| Tensile Strength | ASTM D-1623 | 180 psi |
| Dimensional Stability | 158 F-97% RH for 2 weeks | <1% |
| Water Absorbtion | ASTM D-2842 | <0.5% |
| Water vapor Transmission | ASTM C-355 | 0.5 perms |
| Max Application Temperature | | 250°F |
| Mixing Ratio by Volume | | 1:1AB |
|